- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Self-clinching nuts, studs work in hard sheet materials
- December 24, 2014
- Product Release
- Assembly and Joining
New PEM® self-clinching nuts and studs are available from PennEngineering® for permanent installation into especially hard sheet materials in automotive component attachment applications.
The SH™ hard panel nuts and HFLH™ hard panel studs are manufactured from hardened alloy steel for strong threads. They enable close-to-edge mounting without risking panel buckling. The fasteners eliminate the need for embossing operations, reduce the amount of required hardware in an assembly, and install automatically using a standard press or in-die technology.
The nuts feature a small OD and lightweight design. They can install into high-strength steel sheets at 975-MPa maximum ultimate tensile and in panels as hard as HRC 30/HB 277 or less on the Rockwell C and Brinell scales, respectively
The studs can install into high-strength steel sheets at 700-MPa maximum ultimate tensile and in panels as hard as HRB 96/HB 216 or less on the Rockwell B and Brinell scales, respectively.
Related Companies
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/30/2024
- Running Time:
- 53:00
Seth Feldman of Iowa-based Wertzbaugher Services joins The Fabricator Podcast to offer his take as a Gen Zer...
- Industry Events
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,