- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
30-min. process develops 0.000060-in. black coating
- September 21, 2010
- Product Release
- Finishing
Birchwood Casey offers the scratch-resistant LUMICLAD® finish. The 30-min. process develops a coating thickness of 0.000060 in. with a smooth, clean surface that is electrically conductive and adherent to the aluminum substrate.
The black finish is suitable for precision-machined components with critical dimensions, or for mating surfaces that require break-in lubricity and galling resistance. It has a uniform thickness that will not close down hole diameters or change critical part dimensions.
The coating's inherent lubricity makes it suitable for sliding contacts, such as piston/cylinder assemblies and piston ring grooves. In addition, it is electrically conductive and works well on assemblies requiring a chassis ground.
The patent-pending process delivers a smooth satin black finish with a slightly porous crystal structure that absorbs an optional topcoat, such as clear polymer, light oil, or dry-to-touch sealant. The resulting finish is suitable for aluminum tooling and fixturing devices, sliding assemblies, electronic subframes, and decorative surfaces.
Related Companies
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/30/2024
- Running Time:
- 53:00
Seth Feldman of Iowa-based Wertzbaugher Services joins The Fabricator Podcast to offer his take as a Gen Zer...
- Industry Events
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,