- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Airless, swing-table shotblast system introduced
- February 9, 2010
- Product Release
- Finishing
Viking Blast & Wash Systems has announced the release of the 36 ST airless, swing-table shotblast system.
The worktable is attached to the blast door, so that when the door is opened, the table swings completely clear of the cabinet for loading and unloading. An optional second door with table can be added.
The table rotates while exposed to the abrasive blast, providing a uniform surface finish. The replaceable manganese-alloy steel table liner is 3/8 in. thick and 36 in. in diameter.
The system uses two 5-HP, V10 blast wheels to clean parts up to 28 in. tall and 1,000 lbs. Manganese-alloy plate wear liners protect the blast cabinet in the primary blast zone opposite the blast wheels. Cast chrome liner packages also are available.
Other standard features include an airwash separator for cleaning abrasive before blasting, a separator plate to provide equal distribution of abrasive, and a safety interlock to prevent opening of the blast door during operation.
Related Companies
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/30/2024
- Running Time:
- 53:00
Seth Feldman of Iowa-based Wertzbaugher Services joins The Fabricator Podcast to offer his take as a Gen Zer...
- Industry Events
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,