- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Grinding disks constantly expose fresh abrasives
- October 9, 2007
- Product Release
- Finishing
Flexible, cotton fiber-impregnated abrasive grinding disks from Rex-Cut® Products Inc. have multiple layers of cotton fiber, with the layers fully impregnated with aluminum oxide abrasives and pressed and bonded together to constantly expose fresh abrasives as they work.
The Cut-N-Finish™ disks are suitable for light grinding and blending welds on contoured surfaces. Pressed into a waffle pattern that runs cool, they are offered in a flexible bond that can follow contoured surfaces for the light grinding and blending of GMAW and GTAW welds on tanks and vessels in one step, reports the company.
Capable of producing a 32-RMS finish on stainless steel and nonloading on aluminum, the disks last up to 20 times longer than flap and resin-fiber disks, according to the manufacturer.
Available in flexible and medium bonds with A24, A36, A54, and A80 grit sizes, the disks come in diameters of 4 in., 4 1/2 in., and 7 in. and are suitable for flat surfaces.
Related Companies
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/30/2024
- Running Time:
- 53:00
Seth Feldman of Iowa-based Wertzbaugher Services joins The Fabricator Podcast to offer his take as a Gen Zer...
- Industry Events
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,