- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Laser cutting system designed to provide consistent beam power
- April 15, 2008
- Product Release
- Laser Cutting
Mitsubishi Laser's LVPLUSIIlaser cutting system incorporates 40CF-R resonator technology designed to reduce the rise time and fall time of square wave pulse. The technology is designed to provide consistent beam power during the cutting process and a consistent edge quality. In addition, the uniform, low-current discharge provides low-power stability to help improve micromachining and etching.
The system includes Brilliantcut technology, which is designed to produce a cutting surface roughness equivalent to a typical machined finish, optimize processing conditions, and reduce taper and discoloring on the HAZ.
Jet Pierce technology decreases part time by allowing material to be pierced quickly and aggressively during small-hole processing, the company states. Upgraded height sensor hardware gives the system twice the tracing ability of the company's previous-generation model, the LVPLUS.
The new model is constructed in a heavy-duty, one-piece machine design. A solid Dianite casting provides stability with the machine tool, resonator, and power supply incorporated onto a single platform.
The company's Diamond-Path Technology, which maintains consistent beam quality by using a constant beam length system, provides cutting stability at speeds up to 1,150 IPM across all processing areas. The processing head has multiple features designed to enable high-speed cutting on a range of materials.
The laser cutting system is modular to allow unattended processing. It is available with MELS EYE, an optional intelligent process monitoring system that includes auto focusing, burn detection, pierce detection, and plasma detection.
Related Companies
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/30/2024
- Running Time:
- 53:00
Seth Feldman of Iowa-based Wertzbaugher Services joins The Fabricator Podcast to offer his take as a Gen Zer...
- Trending Articles
JM Steel triples capacity for solar energy projects at Pennsylvania facility
Fabricating favorite childhood memories
How laser and TIG welding coexist in the modern job shop
Robotic welding sets up small-batch manufacturer for future growth
Ultra Tool and Manufacturing adds 2D laser system
- Industry Events
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,