- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Bimetal band saw blades suitable for variety of metals, applications
- October 12, 2004
- Product Release
- Sawing
The L.S. Starrett Co. has introduced the Gladiator™ line of production cutting bimetal band saw blades suitable for a variety of metals and applications.
The blades feature bimetal construction with fatigue-resistant alloy steel backing for durability and heat resistance. The new tooth design features triple-tempered M42 high-speed steel teeth with 8 percent cobalt (HRC 67-69) at up to a 12-degree rake angle. According to the company, the blades are designed to deliver easy penetration; good chip clearance; improved surface finishes; and faster, straighter cuts.
The blades are suitable for high-production cutting in a full range of steels-from mild to stainless, up to 42 HRC-as well as for nickel-based and nonferrous alloys. They come in seven widths and thicknesses, from in. by 0.035 in. to 3 1/8 in. by 0.063 in., and cut a variety of shapes, solids, and tubing.
For large, solid sections of exotic and nickel-based alloys and high-hardness steels, the company also offers Gladiator Pulsator with a specially designed tooth edge that allows the teeth to cut in an aggressive, surging cutting action. These blades come in six different widths and thicknesses, from 1 in. by 0.035 in. to 3 1/8 in. to 0.063 in.
Related Companies
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/30/2024
- Running Time:
- 53:00
Seth Feldman of Iowa-based Wertzbaugher Services joins The Fabricator Podcast to offer his take as a Gen Zer...
- Industry Events
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,