- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Protective packaging prevents corrosion
- April 11, 2006
- Product Release
- Shop Management
Birchwood Casey offers the INTERCEPT® SPS packaging, which provides a protective, corrosion-free zone around metal parts. The packaging material neutralizes and removes corrosive elements in the air around the part as it is stored without the use of chemicals.
The packaging is suitable for all types of products that are shipped overseas or stored for long periods of time indoors or outdoors. The material consists of a polyethylene film infused with metallic copper particles and activated carbon.
These nonhazardous materials neutralize and absorb corrosive elements inside the package through sacrificial galvanic action and absorption. Natural biocides kill acid-producing bacteria, mold, and fungus that may be present inside the package or in fingerprints.
According to the manufacturer, the packaging has a storage life of more than 20 years under normal warehouse conditions. It produces no fumes, no outgassing of volatile organic compounds, and poses no danger of worker sensitivity or allergic reactions.
The packaging is available in presized bags; large, gusseted tote bin-sized bags; shrink film; stretch film; and flat stock.
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/07/2024
- Running Time:
- 67:38
Patrick Brunken, owner of Addison Machine Engineering, joins The Fabricator Podcast to talk about the tube and pipe...
- Industry Events
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,