- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
AISI, STI/SPFA publish steel pipe design manual
- January 15, 2008
- News Release
- Arc Welding
The American Iron and Steel Institute (AISI), Washington, D.C., and the Steel Tank Institute/Steel Plate Fabricators Association (STI/SPFA), Lake Zurich, Ill., jointly published a steel pipe design manual titled Welded Steel Pipe Revised Edition 2007.
The manual focuses on the design of steel pipe up to 240 in. dia. under internal or external pressure. It offers analysis on handling, installation, ring deflection, performance limits, soil mechanics, external loads, coatings, couplings, and other topics. It also includes contributions from experts in the steel water pipe industry.
Targeted to consulting engineers and private/municipal water utility employees, the manual includes technical background and equations that address design issues for water transmission lines and distribution systems that employ welded steel pipe.
The manual is available for download, free of charge, at AISI's Web site (www.steel.org) and the STI/SPFA Web site (www.steeltank.com).
AISI works to advance the case for steel in the marketplace and plays a role in the development and application of new steels and steelmaking technology. STI/SPFA provides a range of services to suppliers and fabricators of steel tanks, pressure vessels, specialty products, and piping for the petroleum, chemical, food, and water storage industries.
Related Companies
subscribe now
The Welder, formerly known as Practical Welding Today, is a showcase of the real people who make the products we use and work with every day. This magazine has served the welding community in North America well for more than 20 years.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/30/2024
- Running Time:
- 53:00
Seth Feldman of Iowa-based Wertzbaugher Services joins The Fabricator Podcast to offer his take as a Gen Zer...
- Industry Events
16th Annual Safety Conference
- April 30 - May 1, 2024
- Elgin,
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI