- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Battery-powered GTAW system offers mobile welding
- April 9, 2015
- Product Release
- Arc Welding
Fronius has introduced the AccuPocket 150/400 battery-powered GTAW system. It offers touchdown ignition, TIG Comfort Stop (TCS), and two- and four-step switchover to facilitate the welding of thin sheets.
The unit’s GTAW pulse function helps reduce heat input, improve gap-bridging ability, and improve weld seam appearance, the company states. It also can be used to achieve a weave pattern in the weld seam typical of GTAW, in which the two components are to be joined without the use of filler metal (autogenous). With the TAC function, the user can join the base material at the start of welding as well as during setting out and tacking.
The machine’s integrated gas solenoid valve provides an optimum gas shield in the start and stop phase. The welding torch has a GTAW multiconnector and built-in up/down switch to help reduce the main current during the welding process. This regulates the heat input and reduces the risk of burn-through.
Related Companies
subscribe now
The Welder, formerly known as Practical Welding Today, is a showcase of the real people who make the products we use and work with every day. This magazine has served the welding community in North America well for more than 20 years.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/30/2024
- Running Time:
- 53:00
Seth Feldman of Iowa-based Wertzbaugher Services joins The Fabricator Podcast to offer his take as a Gen Zer...
- Industry Events
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI