- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
GMAW inverter has built-in programs
- November 11, 2008
- Product Release
- Arc Welding
Miller Electric Mfg. Co.'s Invision 350 MPa GMAW/pulsed-GMAW inverter features built-in programs. The inverter is designed to solve distortion, burn-through, and spatter issues associated with welding light-gauge material. When combined with the S-74 MPa wire feeder, the machines create a synergic system with simplified one-knob control, freeing the operator from setting multiple parameters to achieve optimal results, the company reports. The inverter works with any 14-pin wire feeder.
In pulsed-GMAW mode, the operator dials in the SharpArc (arc cone shape) setting and wire and gas type, and the inverter automatically sets the optimal parameters. Intuitive programming nearly eliminates the pulsed-GMAW learning curve, according to the manufacturer.
The inverter helps provide a controllable arc, even at short arc lengths, for increased precision and productivity. It provides a 5- to 425-amp output (350 amps at 60 percent duty cycle). Incorporating the company's Auto-Line power management technology, the inverter can operate off any input voltage from 208 to 575, single- or three-phase, and provide constant output even if input voltage varies by plusmn; 10 percent, reports the manufacturer.
SharpArc technology alters the width of the pulsed-GMAW arc cone. A low setting produces a wider arc cone that has increased wetting action and weld puddle fluidity, as well as a flatter weld bead. A high setting narrows the arc cone, which produces a narrow weld bead that freezes faster with less heat input.
New technology also lets operators tailor the pulsed-GMAW arc length (voltage) to suit their needs.
Related Companies
subscribe now
The Welder, formerly known as Practical Welding Today, is a showcase of the real people who make the products we use and work with every day. This magazine has served the welding community in North America well for more than 20 years.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/30/2024
- Running Time:
- 53:00
Seth Feldman of Iowa-based Wertzbaugher Services joins The Fabricator Podcast to offer his take as a Gen Zer...
- Industry Events
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,