- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Manual SMAW electrodes introduced
- May 4, 2004
- Product Release
- Arc Welding
The Lincoln Electric Co. has added four new products to its Excalibur® line of all-position, low-hydrogen electrodes for manual SMAW. The electrodes are intended to provide even burnoff, optimum restrike capability and arc stability, less spatter, and easy slag removal, the company says.
The new electrodes are:
- 7018-A1 MR – for all-position welding of 0.50 percent molybdenum low-alloy steels
- 8018-C1 MR – moisture-resistant for welding on equipment and pipe that transport liquid ammonia, propane, and other liquefied gases
- 8018-C3 MR –all-position for fabrication or repair of 1.0 percent nickel steels
- 9018M MR – recommended for use on high-strength steels
The electrodes have a moisture-resistant coating. A square coating burnoff means the arc will not wander and also is resistant to fingernailing in critical out-of-position joints or joints more susceptible to arc blow conditions.
Other features include coating flexibility for less breakage of flux coating when the electrode is bent or when restriking a partially used electrode. According to the company, the electrodes also have less tendency to undercut the weld bead and provide a flat to slightly convex smooth bead profile.
The electrodes are available in 10- and 50-lb. hermetically sealed cans.
Related Companies
subscribe now
The Welder, formerly known as Practical Welding Today, is a showcase of the real people who make the products we use and work with every day. This magazine has served the welding community in North America well for more than 20 years.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/30/2024
- Running Time:
- 53:00
Seth Feldman of Iowa-based Wertzbaugher Services joins The Fabricator Podcast to offer his take as a Gen Zer...
- Trending Articles
The role of flux in submerged arc welding performance
Aluminum MIG wires offer smooth feeding, reduced tangling
Connecticut students compete in Maritime Welding Competition
Three ESAB welding machines win Red Dot Awards for product design
Power source added to cobot welding system for simplified automation
- Industry Events
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,