- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Low-alloy welding wire designed to help improve weld quality on modified Grade 91 steels
- November 8, 2010
- Product Release
- Consumables
To help improve weld quality on modified Grade 91 steels used in high-temperature, high-pressure applications in the power generation and petroleum industries, Hobart Brothers offers its Tri-Mark® TM-B9 welding wire. This gas-shielded, flux-cored wire offers all-position welding capabilities and matches the base material properties.
The wire meets the requirements of chrome-moly welding, including providing an X-factor of less than 15 PPM. The wire also provides a weld deposit with low diffusible hydrogen content — 0.10 fl. oz. per 3.53 oz. of weld metal — to prevent cracking during the pre- and postweld heat-treat cycles of Grade 91 steels. This feature results in X-ray-quality welds and minimizes downtime for rework, the manufacturer states.
The welding wire features a fast-freezing slag that allows for welding in all positions without concern for slag inclusions, according to the company. It also delivers low spatter levels and arc stability.
The wire has a tensile strength of 116 KSI and yield strength of 96 KSI. It is available in 0.045-in. diameters on 33-lb. spools. It operates with a shielding gas mixture of 75 percent argon and 25 percent CO2.
Related Companies
subscribe now
The Welder, formerly known as Practical Welding Today, is a showcase of the real people who make the products we use and work with every day. This magazine has served the welding community in North America well for more than 20 years.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/30/2024
- Running Time:
- 53:00
Seth Feldman of Iowa-based Wertzbaugher Services joins The Fabricator Podcast to offer his take as a Gen Zer...
- Industry Events
16th Annual Safety Conference
- April 30 - May 1, 2024
- Elgin,
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI